TY - CONF A1 - Beckmann, Jörg A1 - Bär, Sylke A1 - Jaunich, Matthias A1 - Wolff, Dietmar A1 - Puskar, L. A1 - Schade, U. T1 - Photolytically and Thermally Initiated Destruction N2 - Casks for storage and transportation of used fuel rods of radioactive material are equipped with polyethylene (PE) for improved neutron flux shielding. The embedded PE structures are additionally exposed to gamma radiation and heat flow due to the specific high activity of the fission products. 60Co γ-radiation and heat load experiments at 125°C has been performed to evaluate PE degradation during the ageing process. FAR-FTIR-experiments were subsequently performed at differently aged PE test samples to characterize the oxidation process and morphological changes in the samples during the ageing at 125°C. T2 - 11'th Joint BER II and BESSY II User Meeting CY - Berlin, Germany DA - 04.12.2019 KW - FTIR KW - High Molecular Polyethylene KW - Ageing PY - 2019 AN - OPUS4-49988 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -