TY - CONF A1 - Kromm, Arne A1 - Thomas, Maximilian A1 - Liepold, Philipp A1 - Kannengießer, Thomas T1 - Increasing the Significance of Varestraint Tests through Improved Crack Evaluation N2 - It was found that there is a systematic dependence of the crack growth on the welding parameters as well as on the load. Decreasing welding speeds with simultaneously higher heat input promote crack formation with increasing strain rate. Based on the results, a new crack criterion was finally selected which allows an extended assessment of the material behavior during the MVT-test. The threshold introduced can quantify the dependencies of the crack formation on the welding and testing parameters, which could not be comprehensively described with the conventional evaluation. In principle, the evaluation routine can also be transferred to other Varestraint or externally loaded hot cracking tests. T2 - IIW Intermediate Meeting Comission II-c CY - Garching, Germany DA - 06.03.2023 KW - Solidification cracking KW - Varestraint-Test PY - 2023 AN - OPUS4-57131 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -