@misc{HaeberleHenkelGargourietal., author = {Haeberle, J{\"o}rg and Henkel, Karsten and Gargouri, Hassan and Naumann, Franziska and Gruska, Bernd and Arens, Michael and Tallarida, Massimo and Schmeißer, Dieter}, title = {Ellipsometry and XPS comparative studies of thermal and plasma enhanced atomic layer deposited Al2O3-films}, series = {Beilstein Journal of Nanotechnology}, volume = {2013}, journal = {Beilstein Journal of Nanotechnology}, number = {4}, issn = {2190-4286}, doi = {10.3762/bjnano.4.83}, pages = {732 -- 742}, abstract = {We report on results on the preparation of thin (<100 nm) aluminum oxide (Al2O3) films on silicon substrates using thermal atomic layer deposition (T-ALD) and plasma enhanced atomic layer deposition (PE-ALD) in the SENTECH SI ALD LL system. The T-ALD Al2O3layers were deposited at 200 °C, for the PE-ALD films we varied the substrate temperature range between room temperature (rt) and 200 °C. We show data from spectroscopic ellipsometry (thickness, refractive index, growth rate) over 4" wafers and correlatethem to X-ray photoelectron spectroscopy (XPS) results. The 200°C T-ALD and PE-ALD processes yield films with similar refractive indices and with oxygen to aluminum elemental ratios very close to the stoichiometric value of 1.5. However, in both also fragments of the precursor are integrated into the film. The PE-ALD films show an increased growth rate and lower carbon contaminations. Reducing the deposition temperature down to rt leads to a higher content of carbon and CH-species. We also find a decrease of the refractive index and of the oxygen to aluminum elemental ratio as well as an increase of the growth rate whereas the homogeneity of the film growth is not influenced significantly. Initial state energy shifts in all PE-ALD samples are observed which we attribute to a net negative charge within the films.}, language = {en} } @misc{HenkelGargouriGruskaetal., author = {Henkel, Karsten and Gargouri, Hassan and Gruska, Bernd and Arens, Michael and Tallarida, Massimo and Schmeißer, Dieter}, title = {Capacitance and conductance versus voltage characterization of Al2O3 layers prepared by PE-ALD at 25°C ≤ T ≤ 200°C}, series = {Journal of Vacuum Science and Technology A}, volume = {1}, journal = {Journal of Vacuum Science and Technology A}, number = {32}, doi = {10.1116/1.4831897}, pages = {01A107-1 -- 01A107-10}, abstract = {In this work, plasma enhanced atomic layer deposited (PE-ALD) samples were prepared at substrate temperatures in the range between room temperature (RT) and 200 °C and investigated by capacitance-voltage and conductance-voltage recordings. The measurements are compared to standard thermal atomic layer deposition (T-ALD) at 200 °C. Very low interface state density (D it) ~1011 eV-1 cm-2 could be achieved for the PE-ALD process at 200 °C substrate temperature after postdeposition anneal (PDA) in forming gas at 450 °C. The PDA works very effectively for both the PE-ALD and T-ALD at 200 °C substrate temperature delivering also similar values of negative fixed charge density (N fix) around -2.5 × 1012 cm-2. At the substrate temperature of 150 °C, highest N fix (-2.9 × 1012 cm-2) and moderate D it (2.7 × 1011 eV-1 cm-2) values were observed. The as deposited PE-ALD layer at RT shows both low D it in the range of (1 to 3) × 1011 eV-1 cm-2 and low N fix (-4.4 × 1011 cm-2) at the same time. The dependencies of N fix, D it, and relative permittivity on the substrate temperatures and its adjustability are discussed.}, language = {en} } @inproceedings{HenkelTallaridaHaeberleetal., author = {Henkel, Karsten and Tallarida, Massimo and Haeberle, J{\"o}rg and Gargouri, Hassan and Naumann, Franziska and Gruska, Bernd and Arens, Michael and Schmeißer, Dieter}, title = {PE-ALD-Al2O3-Schichten f{\"u}r die Passivierung von Solarzellen}, series = {Tagungsband Photovoltaik-Meeting: Anwendungen-Qualit{\"a}t-Perspektiven, Senftenberg, 16.04.2014}, booktitle = {Tagungsband Photovoltaik-Meeting: Anwendungen-Qualit{\"a}t-Perspektiven, Senftenberg, 16.04.2014}, editor = {Gl{\"u}ck, Bernhard K. and Schmidt, Sindy and Stein, Erhard and Raschke, J{\"o}rg-Uwe and Richter, Hans}, publisher = {Cottbus-Senftenberg}, address = {BTU}, pages = {7 -- 14}, abstract = {D{\"u}nne Al2O3-Schichten wurden bei Substrattemperaturen zwischen Raumtemperatur und 200°C mittels PE-ALD auf Si-Substraten abgeschieden und ellipsometrisch, spektroskopisch und elektrisch charakterisiert. Ihr Potenzial f{\"u}r die chemische und Feldeffektpassivierung der Oberfl{\"a}chenrekombination wird bewertet.}, language = {de} } @misc{DasHenkelTallaridaetal., author = {Das, Chittaranjan and Henkel, Karsten and Tallarida, Massimo and Schmeißer, Dieter and Gargouri, Hassan and K{\"a}rkk{\"a}nen, Irina and Schneidewind, Jessica and Gruska, Bernd and Arens, Michael}, title = {Thermal and plasma enhanced atomic layer deposition of TiO2: Comparison of spectroscopic and electric properties}, series = {Journal of Vacuum Science and Technology A}, volume = {2015}, journal = {Journal of Vacuum Science and Technology A}, number = {33}, issn = {1520-8559}, doi = {10.1116/1.4903938}, pages = {01A144-1 -- 01A144-8}, abstract = {Titanium oxide (TiO2) deposited by atomic layer deposition (ALD) is used as a protective layer in photocatalytic water splitting system as well as a dielectric in resistive memory switching. The way ALD is performed (thermally or plasma-assisted) may change the growth rate as well as the electronic properties of the deposited films. In the present work, the authors verify the influence of the ALD mode on functional parameters, by comparing the growth rate and electronic properties of TiO2 films deposited by thermal (T-) and plasma-enhanced (PE-) ALD. The authors complete the study with the electrical characterization of selected samples by means of capacitance-voltage and current-voltage measurements. In all samples, the authors found a significant presence of Ti3+ states, with the lowest content in the PE-ALD grown TiO2 films. The observation of Ti3+ states was accompanied by the presence of in-gap states above the valence band maximum. For films thinner than 10 nm, the authors found also a strong leakage current. Also in this case, the PE-ALD films showed the weakest leakage currents, showing a correlation between the presence of Ti3+ states and leakage current density.}, language = {en} } @inproceedings{HenkelDasSowinskaetal., author = {Henkel, Karsten and Das, Chittaranjan and Sowinska, Małgorzata and Tallarida, Massimo and Schmeißer, Dieter and Gargouri, Hassan and K{\"a}rkk{\"a}nen, Irina and Schneidewind, Jessica and Gruska, Bernd and Arens, Michael}, title = {Charakterisierung von TiO2-ALD-Schichten und deren Nutzung f{\"u}r die Passivierung von Si-Photokathoden}, series = {Tagungsband Photovoltaik-Meeting: Anwendungen-Qualit{\"a}t-Perspektiven, Senftenberg, 15.04.2015}, booktitle = {Tagungsband Photovoltaik-Meeting: Anwendungen-Qualit{\"a}t-Perspektiven, Senftenberg, 15.04.2015}, editor = {Gl{\"u}ck, B. K. and Schmidt, S. and Stein, E. and Raschke, J{\"o}rg-Uwe and Richter, H.}, publisher = {BTU Cottbus-Senftenberg}, address = {Senftenberg}, pages = {3 -- 8}, abstract = {Wir berichten zun{\"a}chst {\"u}ber den Einfluss der Methode der Atomlagenabscheidung auf die TiO2-Schichteigenschaften. Insbesondere wird der Zusammenhang zwischen Ti3+- sowie Interbandzust{\"a}nden mit elektrischen Kennlinien und deren Einfluss auf funktionale Schichteigenschaften diskutiert. Anschließend werden Mikrostrukturierung, Grenzfl{\"a}chen-Engineering und konforme Abscheidung einer TiO2-ALD-Schutzschicht effektiv zur Performance-Steigerung von p-Si-Photokathoden angewendet.}, language = {de} }